MIL-T-9046 AB-2 6AL-4V ELI

MIL-T-9046
Revision: “J” issued 01/1983 ***Obsolete, S/S by AMS-T-9046***
Alloy: 6AL-4V “AB-2”
Product Forms: Titanium and Titanium Alloy, Sheet, Strip, and Plate
Condition: Annealed

Please note, the MIL-T-9046 specification covers various Alloys and Conditions. This Spec Sheet is only for the Alloy and Condition listed above.

Composition Analysis
Aluminum: 5.5 – 6.5% Nitrogen (Maximum): 0.05%
Vanadium: 3.5 – 4.5% Hydrogen (Maximum): 0.0125%
Iron (Maximum): 0.25% Other Elements (Total): 0.30%
Oxygen (Maximum): 0.13% Titanium: Balance
Carbon (Maximum): 0.08%

 

Tensile Properties (Minimums)*
Tensile: 125 – 130 ksi Elongation: 6 – 10%
Yield: 115 – 120 ksi

*Tensile property requirements vary based on orientation, section thickness, and cognizant engineering organization requirements.

Required Acceptance Tests

  • Chemical Composition
  • Microstructure
  • Ultrasonic (where required)
  • Tensile Properties
  • Bend Test (where required)

Disclaimer
The use of this information is strictly voluntary. Information may contain typographical errors, and should be used as a guideline only. This Material Spec Sheet contains generalizations and is in no way a substitution for the MIL-T-9046 specification.

To download MIL-T-9046J, please visit: https://assist.dla.mil/online/start/

Changes may be made to the information contained herein.

PERFORMANCE TITANIUM GROUP: A CUT ABOVE THE REST