AMS 6936
AMS 6936
Revision: “D” issued 11/2023
Alloy: 6AL-6V-2SN
Product Forms: Titanium Bars, Forgings, and Forging Stock
Condition: Annealed
Composition Analysis | |
---|---|
Aluminum: 5.0 – 6.0% | Carbon (Maximum): 0.05% |
Vanadium: 5.0 – 6.0% | Nitrogen (Maximum): 0.04% |
Tin: 1.5 – 2.5% | Hydrogen (Maximum): 0.015% |
Iron: 0.35 – 1.0% | Yttrium (Maximum): 0.005% |
Copper: 0.35 – 1.0% | Other Elements (Total): 0.30% |
Oxygen (Maximum): 0.20% | Titanium: Balance |
Tensile Properties (Minimums)* | |
---|---|
Tensile: 137 – 148 ksi | Elongation: 8 – 10% |
Yield: 129 – 137 ksi | Reduction of Area: 15 – 20% |
*Tensile property requirements vary based on orientation, section thickness/diameter, and cognizant engineering organization requirements.
Required Acceptance Tests
- Chemical Composition
- Tensile Properties
- Microstructure
- Surface Contamination
- Macrostructure
- Ultrasonic (where required)
Disclaimer
The use of this information is strictly voluntary. Information may contain typographical errors, and should be used as a guideline only. This Material Spec Sheet contains generalizations and is in no way a substitution for the AMS 6936 specification.
To purchase AMS 6936D, please visit: https://www.sae.org/standards/content/ams6936d/