AMS 4978
AMS 4978
Revision: “J” issued 05/2022
Alloy: 6AL-6V-2SN
Product Forms: Titanium Bars, Forgings, and Rings
Condition: Annealed
Composition Analysis | |
---|---|
Aluminum: 5.0 – 6.0% | Carbon (Maximum): 0.05% |
Vanadium: 5.0 – 6.0% | Nitrogen (Maximum): 0.04% |
Tin: 1.5 – 2.5% | Hydrogen (Maximum): 0.015% |
Iron: 0.35 – 1.0% | Yttrium (Maximum): 0.005% |
Copper: 0.35 – 1.0% | Other Elements (Total): 0.40% |
Oxygen (Maximum): 0.20% | Titanium: Balance |
Tensile Properties (Minimums)* | |
---|---|
Tensile: 145-150 ksi | Elongation: 8 – 10% |
Yield: 135-165 ksi | Reduction of Area: 15 – 20% |
*Tensile property requirements vary based on orientation, section thickness/diameter, and cognizant engineering organization requirements.
Required Acceptance Tests
- Tensile Properties
- Microstructure
- Surface Contamination
- Fracture Toughness (when specified)
- Chemical Composition
Disclaimer
The use of this information is strictly voluntary. Information may contain typographical errors, and should be used as a guideline only. This Material Spec Sheet contains generalizations and is in no way a substitution for the AMS 4978 specification.
To purchase AMS 4978J, please visit: http://standards.sae.org/ams4978j/
Changes may be made to the information contained herein.