AMS 4965
Revision: “N” issued 08/2022
Alloy: 6AL-4V
Product Forms: Titanium Alloy, Bars, Wire, Forgings, and Rings
Condition: Solution Heat Treated and Aged
| Composition Analysis | |
|---|---|
| Aluminum: 5.5 – 6.75% | Nitrogen (Maximum): 0.05% |
| Vanadium: 3.5 – 4.5% | Hydrogen (Maximum): 0.0125% |
| Iron (Maximum): 0.30% | Yttrium (Maximum): 0.005% |
| Oxygen (Maximum): 0.20% | Other Elements (Total): 0.40% |
| Carbon (Maximum): 0.08% | Titanium: Balance |
| Tensile Properties (Minimums)* | |
|---|---|
| Tensile: 130 – 165 ksi | Elongation: 6 – 10% |
| Yield: 120 – 155 ksi | Reduction of Area: 20 – 25% |
*Tensile property requirements vary based on orientation, section thickness/diameter, and cognizant engineering organization requirements.
Required Acceptance Tests
- Chemical Composition
- Tensile Properties
- Microstructure
- Surface Contamination
- Fracture Toughness (when specified)
Disclaimer
The use of this information is strictly voluntary. Information may contain typographical errors, and should be used as a guideline only. This Material Spec Sheet contains generalizations and is in no way a substitution for the AMS 4965 specification.
To purchase AMS 4965N, please visit: https://www.sae.org/standards/content/ams4965n/
Changes may be made to the information contained herein.