AMS 4930
Revision: “-M” issued 11/2025
Alloy: 6AL-4V Eli
Product Forms: Titanium Alloy Bars, Wire, Forgings, and Rings
Condition: Annealed
| Composition Analysis | |
|---|---|
| Aluminum: 5.5 – 6.5% | Nitrogen (Maximum): 0.05% |
| Vanadium: 3.5 – 4.5% | Hydrogen (Maximum): 0.0125% |
| Iron (Maximum): 0.25% | Other Elements (Each): .10% |
| Oxygen (Maximum): 0.13% | Other Elements (Total): .40% |
| Carbon (Maximum): 0.08% | Titanium: Balance |
| Tensile Properties (Minimums)* | |
|---|---|
| Tensile: 117 – 125 ksi | Elongation: 8 – 10% |
| Yield: 108 – 115 ksi | Reduction of Area: 15 – 25% |
*Tensile property requirements vary based on orientation, section thickness/diameter, and cognizant engineering organization requirements.
Required Acceptance Tests
- Chemical Composition
- Tensile Properties
- Microstructure
- Surface Contamination
Disclaimer
The use of this information is strictly voluntary. Information may contain typographical errors, and should be used as a guideline only. This Material Spec Sheet contains generalizations and is in no way a substitution for the AMS 4930 specification.
To purchase AMS 4930M, please visit: http://standards.sae.org/ams4930m/