AMS 4907

AMS 4907
Revision: “-M” issued 08/2020
Alloy: 6AL-4V Eli
Product Forms: Titanium Alloy, Sheet, Strip, and Plate
Condition: Annealed

Composition Analysis
Aluminum: 5.5 – 6.5% Nitrogen (Maximum): 0.05%
Vanadium: 3.5 – 4.5% Hydrogen (Maximum): 0.0125%
Iron (Maximum): 0.25% Other Elements (Each): .10%
Oxygen (Maximum): 0.13% Other Elements (Total): .40%
Carbon (Maximum): 0.08% Titanium: Balance
Yttrium (Maximum): .005%

 

Tensile Properties (Minimums)*
Tensile: 125 – 130 ksi Elongation: 6 – 10%
Yield: 115 – 120 ksi

*Tensile property requirements vary based on orientation, section thickness, and cognizant engineering organization requirements.

Required Acceptance Tests

  • Chemical Composition
  • Tensile Properties
  • Bend Test (where required)
  • Microstructure
  • Surface Contamination

Disclaimer
The use of this information is strictly voluntary. Information may contain typographical errors, and should be used as a guideline only. This Material Spec Sheet contains generalizations and is in no way a substitution for the AMS 4907 specification.

To purchase AMS 4907M, please visit: http://standards.sae.org/ams4907m/

Changes may be made to the information contained herein.

PERFORMANCE TITANIUM GROUP: A CUT ABOVE THE REST