AMS 4967

AMS 4967
Revision: “N” issued 08/2022
Alloy: 6AL-4V
Product Forms: Titanium Alloy, Bars, Wire, Forgings, and Rings
Condition: Annealed, Heat Treatable

Composition Analysis
Aluminum: 5.5 – 6.75% Nitrogen (Maximum): 0.05%
Vanadium: 3.5 – 4.5% Hydrogen (Maximum): 0.0125%
Iron (Maximum): 0.30% Yttrium (Maximum): 0.005%
Oxygen (Maximum): 0.20% Other Elements (Total): 0.40%
Carbon (Maximum): 0.08% Titanium: Balance

 

Tensile Properties (Minimums)*
Tensile: 130 – 165 ksi Elongation: 6 – 10%
Yield: 120 – 155 ksi Reduction of Area: 20 – 25%

*Tensile property requirements vary based on orientation, section thickness/diameter, and cognizant engineering organization requirements.

Required Acceptance Tests

  • Chemical Composition
  • Tensile Properties (after Heat Treat)
  • Microstructure
  • Surface Contamination

Disclaimer
The use of this information is strictly voluntary. Information may contain typographical errors, and should be used as a guideline only. This Material Spec Sheet contains generalizations and is in no way a substitution for the AMS 4967 specification.

To purchase AMS 4967N, please visit: https://www.sae.org/standards/content/ams4967n/

Changes may be made to the information contained herein.

PERFORMANCE TITANIUM GROUP: A CUT ABOVE THE REST